Guided wave testing (GWT) is a non-destructive evaluation method. The methodemploys acoustic waves that propagate along an elongatedstructure while guided by its boundaries. This allows thewaves to travel a long distance with little loss in energy. Nowadays, GWT is widely used to inspect and screen manyengineering structures, particularly for the inspectionof metallic pipelines around the world. Insome cases, hundreds of meters can be inspected from a singlelocation. There are also some applications for inspectingrail tracks, rods and metal plate structures.
Although guided wave testing is also commonly known as guided waveultrasonic testing (GWUT) or ultrasonic guided waves (UGWs) or long range ultrasonic testing (LRUT),it is fundamentally very different fromconventional ultrasonic testing. The frequency used in the inspection depends on the thickness of the structure, but guided wavetesting typically uses ultrasonic frequencies in the range of 10 kHz to several MHz.Higher frequencies can be used in some cases, but detection range is significantly reduced. In addition, the underlying physics of guided waves is morecomplex than bulk waves. Much of the theoretical background hasbeen addressed in a separate article. In thisarticle, the practical aspect of GWT will be discussed.
- 4Features
History[edit]
The study of guided waves propagating in a structure can betraced back to as early as the 1920s, mainly inspired by the fieldof seismology. Since then, there has been an increased effort onthe analytical study of guided wave propagation in cylindricalstructures. It was only in the early 1990s that guided wave testing wasconsidered as a practical method for the non-destructive testing of engineeringstructures. Today, GWT is applied as an integrated healthmonitoring program in the oil, gas and chemical industries.
![Pipeline Pipeline](http://www.sunnysteel.com/images/ultrasonic-test-on-astm-a335-p22-pipe.jpg)
Ultrasonic Pipe / Tank Testing ULTRASONIC PIPE TESTING Due to the combination of a wide variety of physical factors, building operations and management personnel are finding themselves faced with new and more complex corrosion related piping problems. Many are clearly related to the quality of the water treatment program or a past lack of.
How it works (pipeline inspections)[edit]
Unlike conventional ultrasonics, there are an infinite number ofguided wave modes that exist for a pipe geometry, and they can begenerally grouped into three families, namely the torsional,longitudinal and flexural modes. The acoustic properties of thesewave modes are a function of the pipe geometry, the material and thefrequency. Predicting theseproperties of the wave modes often relies on heavy mathematical modeling which are typicallypresented in graphical plots called dispersioncurves.
In guided wave testing of pipelines, an array of low frequencytransducers is attached around the circumference of the pipe to generatean axially symmetric wave that propagates along the pipe in both the forward and backwarddirections of the transducer array. The Torsional wave mode is most commonlyused, although there is limited use of the longitudinal mode. The equipment operates in a pulse-echoconfiguration where the array of transducers is used for both theexcitation and detection of the signals.
At a location where there is a change of cross-section or a change inlocal stiffness of the pipe, an echo is generated. Based on thearrival time of the echoes, and the predicted speed of the wave mode at aparticular frequency, the distance of a feature in relation to theposition of the transducer array can be accurately calculated. GWTuses a system of distance amplitude curves (DAC) to correct forattenuation and amplitude drops when estimating the cross-sectionchange (CSC) from a reflection at a certain distance. The DACs areusually calibrated against a series of echoes with known signalamplitude such as weld echoes.
Once the DAC levels are set, the signal amplitude correlates well to the CSC of a defect. GWT does not measure theremaining wall thickness directly, but it is possible to group thedefect severity in several categories. One method of doing this isto exploit the mode conversion phenomenon of the excitation signalwhere some energy of the axially symmetric wave mode is converted tothe flexural modes at a pipe feature. Theamount of mode conversion provides an accurate estimate of thecircumferential extent of the defect, and together with the CSC,operators could establish the severity category.
A typical result of GWT is displayed in an A-scan style with thereflection amplitude against the distance from the transducer array position.In the past few years, some advanced systems have started to offerC-scan type results where the orientation of each feature canbe easily interpreted. This has shown to be extremely useful wheninspecting large size pipelines.
Guided wave focusing[edit]
As well as incorporating C-scan type results, active focusing capacity can also be achieved by GWT utilising flexural wave modes. This gives two main advantages; firstly the signal to noise ratio (SNR) of a defect echo can be enhanced, secondly it can be used as an additional tool to help discriminate between 'real' and 'false' indications. However, there are disadvantages associated with this technique; firstly, the defect location must be known before the focusing can be applied, secondly, the separate data set required for the active focusing technique can also significantly reduce the time and cost efficiency of GWT.
Flexural wave modes have sinusoidal variation in their displacement pattern around the circumference, in integer values ranging from 1 to Infinity. Active focusing involves the transmission of multiple flexural wave modes, with time and amplitude corrections applied, in such a way that a circumferential node from each wave mode will arrive at the target position at the same time, the same circumferential position and with the same phase, causing constructive interference. At other circumferential positions the circumferential nodes of the flexural wave modes will arrive out of phase with each other and will interfere destructively. Adjusting the excitation conditions can rotate this focal spot around the pipes circumference. Comparing the response from different circumferential positions can allow the operator to more accurately predict the circumferential position and extent of a defect.
As previously mentioned, the focusing technique can also be used to help discriminate between 'real' and 'false' indications, a 'false' indication being a received signal that does not directly correspond to the position of a defect; such as those from reverberations or from incomplete cancellation of unwanted wave modes. If a 'false' indication is present in the A-scan data, it will also be re-represented in any C-scan type results as this type of processing uses the same original data. As active focusing involves a separate data collection, focusing at the position of a 'false' indication will give a negative result, whereas focusing on a 'true' indication will give a positive result. Therefore, the active focusing technique can help overcome the propensity of 'false calls' generated by guided wave testing systems.
Features[edit]
Advantages[edit]
- Rapid screening for in-service degradation (Long range inspection) – potential to achieve hundreds of meters of inspection range.
- Detection of internal or external metal loss
- Reduction in costs of gaining access – insulated line with minimal insulation removal, corrosion under supports without need for lifting, inspection at elevated locations with minimal need for scaffolding, and inspection of road crossings and buried pipes.
- Data is fully recorded.
- Fully automated data collection protocols.
Disadvantages[edit]
- Interpretation of data is highly operator dependent.
- Difficult to find small pitting defects.
- Not very effective at inspecting areas close to accessories.
- Needs good procedure
List of standards[edit]
- British Standards (BSI)
![Ultrasonic pipe inspection equipment Ultrasonic pipe inspection equipment](https://irp-cdn.multiscreensite.com/2129f79d/dms3rep/multi/mobile/Billet+Inspection+System.png)
- BS 9690-1:2011, Non-destructive testing. Guided wave testing. General guidance and principles
- BS 9690-2:2011, Non-destructive testing. Guided wave testing. Basic requirements for guided wave testing of pipes, pipelines and structural tubulars
- ASTM International (ASTM)
- E2775 – 16, Standard Practice for Guided Wave Testing of Above Ground Steel Pipework Using Piezoelectric Effect Transduction
- E2929 – 13, Standard Practice for Guided Wave Testing of Above Ground Steel Piping with Magnetostrictive Transduction